Castrol superclean damages



In response to the lister advising against super clean.

I recommend NOT using super clean on any surface made of aluminum or
coated items. Further, it is not as non toxic as people may think (usually
people associate toxicity with volatility).

Super clean is made from sodium hydroxide, NaOH. This is a very strong
base, despite some dilution. I use sodium hydroxide as an etchant for
aluminum pieces in preparation for plating and anodization. Very harsh on
aluminum. Red Devil drain opener has this base, but in powdered form.
Heats up on contact with water. If anyone wants to experiment, make a
solution of Red Devil and water, insert an empty soda can. Come back 1/2
hour later.

NaOH will remove any type of color and hard anodization. You can use it
for a few minutes, but do ya wanna take a chance? I took a chance on my
very expensive mountain bike's very expensive hard anodized chainrings.
Faded the anodization and the teeth are wearing fast. Some have
recommended this stuff for intercoolers and radiators. Very bad. Use
Simple green or a petroleum based cleaner/solvent.

****************************************************************************
*Steve                                             Sachelle Babbar
*'87  5000CS Turbo 5spd 1.3-2.0 bar             <SBABBAR@IRIS.NYIT.EDU>
*Cockpit adjustable wastegate, AudiSport badge
*
*Disclaimer:"Any information contained herein is based purely on my own
*personal experience and may not necessarily reflect yours. Use caution as